Type: | Ceramic Parts | Application: | Structure Ceramic, Industrial Equipment |
---|---|---|---|
Material: | Alumina Ceramic | Processing Service: | Custom Processing |
Product Name: | Precision Ceramic Parts | Color: | Customizable |
Size: | Customized Size | Material Option: | Customizable |
Production Methods: | According To Drawing | Drawing Format: | 2D/(PDF/CAD)3D(IGES/STEP) |
Advantage: | High Precision | Quality Control: | 100% Inspection |
Port: | Shenzhen Or Hong Kong | ||
High Light: | Microporous Alumina Ceramic Membranes 3.9g Cm3 BPT,alumina filter membrane BPT,Tubular Porous Alumina Ceramic Membranes 3.9g Cm3 BPT |
Description of high purity alumina ceramic rods
Al2O3 ceramic rod gets an excellent corrosion resistance, high insulation, exceptional mechanical strength. Long-term sunshine, rainfall, humidity or other weather factors do little effect and damage on the rod surface, not even ultraviolet rays can change the rod surface quality. Meanwhile, the alumina rod has acid and alkali stability, thermal stability, high machining strength, and hardness. These advantages make sure that the alumina rod is competent in severe operating conditions.
Our company supplies a great of dense alumina rod made of high purity material, of what the performance and parameter reach to the international level, we also supply polishing and glazing treatment on the rod surface, which make rods smooth and enhance its performance in the application.
Alumina ceramic performance table
|
|||||
Property
|
Item
|
Data
|
Unit
|
||
99.8% | 99% | 95% | |||
Mechanical Characteristics
|
color | Ivory | light yellow | White | - |
density | 3.93 | 3.85 | 3.7 | g/cm3 | |
Bending Strength | 370 | 310 | 300 | MPa | |
Compressive trength | 2,500 | 2,400 | 2,300 | MPa | |
Elastic Modulus | 390 | 340 | 320 | GPa | |
Fracture Toughness | 4 | 3~4 | 3~4 |
MPa m^1/2
|
|
Weber Coefficient | 12 | 12 | 12 | m | |
Vickers Hardness | 1,850 | 1,600 | 1,400 | HV 0.5 | |
Thermal Characterics
|
Coefficient of Line Thermal
Expansion
|
7~8 | 7~8 | 7~8 |
10^-6 K^-1
|
Thermal Conductivity
|
32 | 29 | 20 |
W/mK
|
|
Thermal Shock Resistance
(Put in Water)
|
280 | 200 | 250 | ΔT °C | |
Max Working Temperature
|
1,700 | 1,600 | 1,500 | °C | |
Electrical Characteristics
|
Volume Resistance at 20°C
|
>10^14 | >10^14 | >10^14 | Ωcm |
Dielectric Strength
|
15×10^6
|
15×10^6
|
15×10^6
|
V/m
|
|
Dielectric Constant | 10 | 10 | 10 | εr | |
One MHZ Dielectric Loss Angle
at 20°C
|
0.0001 |
0.0002
|
0.0004 |
tanδ
|
|
Chemical Characteristics
|
Nitric Acid (60%) 90°C
|
0.05 | 0.1 | 0.1 |
WT Loss mg/cm^2/day
|
Sulphuric Acid (95%) 95°C | 0.22 | 0.34 | 0.3 | ||
Caustic Soda (30%) 80°C
|
0.04 | 0.95 | 0.9 |